Master Bond Product Search

357 products match

EP33CLV Two Part Epoxy EP33CLV

Room temperature curing epoxy adhesive features high thermal stability. Excellent chemical resistance properties. High bond strength. Volume resistivity o >1014 ohm-cm. Withstands thermal cycling. Serviceable from -60°F to +450°F. Successfully tested for 1,000 hours 85°C/85% RH. One to one mix ratio by volume. Low viscosity.

EP33LV Two Part Epoxy EP33LV

Convenient one to one mix ratio by volume. Service temperature range -60°F to +450°F. Cures at room temperature. Moderate viscosity. Outstanding dimensional stability. Reliable electrical insulator. Robust chemical resistance.

EP33ND Two Part Epoxy EP33ND

Non-drip thixotropic epoxy paste. Demonstrated radiation stability at high radiation dosages. Serviceable from -60°F to +450°F. Gap filling. One to one mix ratio by volume. Adheres well to similar and dissimilar substrates. Cures at ambient temperatures. Post cure to optimize properties. Readily machinable.

EP34 Two Component Epoxy EP34

Two component, high temperature resistant epoxy adhesive, sealant, coating. Top notch electrical insulator. Dimensionally stable. Easily machinable. High strength system. Service temperature range from -60°F to +450°F.

EP34AN Two Part Epoxy System EP34AN

Exceptionally high thermal conductivity. Superb electrical insulation properties. Serviceable from -60°F to +450°F. Paste viscosity. Can be applied on vertical surfaces without dripping. Gap filling. Low CTE. Excellent dimensional stability.

EP34AN-1 Two Part Epoxy EP34AN-1

Thermally conductive/electrically insulative thixotropic paste. Service temperature range -60°F to +450°F. Ability to withstand thermal cycling. Bonds well to similar and dissimilar substrates. Gap filler.

EP34AO Two Part Epoxy System EP34AO

Thermally conductive, electrically insulative, room temperature curing epoxy system. High bond strength. Thermal stability. Superior chemical resistant properties. Paste viscosity. Gap filling. Low shrinkage. Superb electrical insulation characteristics. Serviceable from -60°F to +450°F.

EP34CA Two Part Epoxy EP34CA

Resists -80°F to +500°F. Two component epoxy system. Long open time. Good flow properties. Can cure in section exceeding 1/4 inch thick. Withstands 1,000 hours 85°C/85% RH. Protects against aggressive chemical exposure.

EP34LV Two Part Epoxy EP34LV

Two part moderate viscosity epoxy adhesive, sealant, coating. Features high temperature resistance. Superb electrical insulation properties. Service temperature range -60°F to +450°F. Excellent bond strength. Easily machinable. Successfully tested for 1,000 hours 85°C/85% RH.

EP35 Two Part Epoxy EP35

High viscosity epoxy adhesive offers excellent thermal stability. Serviceable from -60°F to +450-500°F. Durable. High strength bonds are maintained even after long-term exposures to elevated temperatures. Outstanding resistance to chemical exposure.