EP112LS Two Part Heat Curing Epoxy EP112LS

Potting, encapsulation, sealing and impregnation compound. Low viscosity two component epoxy system. Heat curable. Long working life at room temperature. Superb optical clarity. Non-yellowing. Serviceable from -60°F to +450°F. High dielectric strength.

EP112M Two Component Epoxy EP112M

Medium viscosity heat curing cycloaliphatic epoxy resin system. Outstanding arc, corona and tracking resistance. Excellent dielectric properties. Resilient. Good endurance in outdoor/indoor environments. High bond strength. Low shrinkage. Serviceable from -60°F to +500°F.

EP113 Two Component Epoxy EP113

Two component nanosilica filled epoxy for potting, coating and sealing. Optically clear. Low shrinkage. Superior electrical insulation properties. Toughened system. Successfully tested for 1,000 hours 85°C/85% RH. Serviceable from -100°F to +450°F.

EP114 Two Component Epoxy EP114

Two component nanosilica filled epoxy for potting, coating and sealing. Optically clear. Low shrinkage. Superior electrical insulation properties. Toughened system. Successfully tested for 1,000 hours 85°C/85% RH. Serviceable from -100°F to +450°F.

EP121AO Two Part Epoxy EP121AO

Thermally conductive, electrically insulative. Long working life. Outstanding dimensional stability. Superb heat resistance. Low coefficient of thermal expansion. Passes NASA low outgassing tests. Very long open time. Ideally suited for potting applications. Serviceable from -60°F to +500°F. Medium viscosity.

EP121CL Two Part Epoxy System EP121CL

Low viscosity epoxy with an extraordinary long open time. Superior dielectric strength. Impressive optical clarity. Excellent chemical resistance. Serviceable from -80°F to +500°F.

EP121CL-LO Two Part Epoxy EP121CL-LO

NASA low outgassing approved two component epoxy. Low viscosity system. High dielectric strength. Optically clear. Withstands 1,000 hours 85°C/85% RH. Shore D hardness 80-90. Serviceable from -80°F to +500°F. Long open time at room temperature.

EP125 Two Component Epoxy EP125

Structural epoxy adhesive resists temperatures up to 500°F. Exceptional durability and flexural strength. High adhesion to metallic and non-metallic substrates. Heat curable system. Tg +240°C. Special two part epoxy with very long working life. Excellent compressive strength. Service operating temperature range from -80°F to +600°F.

EP13 One Part Epoxy System EP13

One component, heat curable epoxy adhesive. Serviceable from -60°F to +500°F. Paste viscosity. High tensile shear and compressive strength. Chemical resistant. Machinable.

EP132 Two Part Epoxy EP132

Two part high temperature resistant epoxy system. Capable of service up to 550°F. 100% reactive. Unmatched durability. Outstanding electrical and physical strength properties. Service operating temperature range from -60°F to +550°F.