EP30AOHT Two Part Epoxy EP30AOHT

Thermal conductive/electrically insulative epoxy for bonding, potting, sealing, coating. Serviceable from -60°F to +400°F. Low CTE. Rigid bonds. Excellent dielectric strength. Flowable.

EP30AOSP Two Part Epoxy EP30AOSP

Room temperature curing epoxy. Thermally conductive/electrical insulative. Low viscosity with excellent flowability. Suitable for potting and casting. Outstanding chemical resistance. Shore D hardness 90. High compressive strength. Serviceable from -60°F to +250°F.

EP30D-10 Urethane Modified Epoxy System EP30D-10

Optically clear, elastomeric system. Urethane modified epoxy. 100% reactive. Serviceable from -100°F to 220°F. Long working life. Resistant to thermal cycling. High impact strength. Outstanding flexibility. Protects against abrasion. Minimal linear shrinkage upon cure. Low moisture permeability.

EP30D-7 Two Part Urethane Modified Epoxy System EP30D-7

Urethane-modified epoxy system. Superior toughness and abrasion resistance. Cures at room temperatures. Compound flows easily and smoothly. Versatile cure schedule.

EP30D-7SPHT

Urethane-modified epoxy system. Superior toughness and abrasion resistance. Cures at room temperatures. Compound flows easily and smoothly. Versatile cure schedule.

EP30DP Two Part Epoxy EP30DP-NV

Two part, room temperature curing, lower viscosity system used primarily for potting and encapsulation applications. Excellent thermal cycling properties along with shock and vibration resistance. Low exotherm and long working life. Superb abrasion resistance and electrical insulation characteristics. Repairable. Serviceable from 4K to +250°F.

EP30DPMed Two Component Epoxy-Urethane Blended System EP30DPBFMed

Epoxy-urethane blend. Superior toughness and abrasion resistance. Biocompatible. Cryogenically serviceable. Low viscosity. Low moisture absorption and hydrolytic stability. USP Class VI approved. Serviceable from 4k to +250°F. Outstanding electrical insulation properties. Withstands thermal cycling. High impact strength.

EP30DPSP Two Part Epoxy EP30DPSP

Epoxy-urethane blend. Superior toughness and abrasion resistance. Biocompatible. Cryogenically serviceable. Low viscosity. Low moisture absorption and hydrolytic stability. USP Class VI approved. Serviceable from 4k to +250°F. Outstanding electrical insulation properties. Withstands thermal cycling. High impact strength.

EP30F Two Component Epoxy EP30F
EP30FL Two Part Epoxy EP30FL

Low viscosity, optically clear epoxy. Ideal for thermal cycling and bonding sensitive components. Room temperature or low elevated temperature cure. Good flexibility. Superb impact resistance. Shore D hardness 25-40. Serviceable from 4k to +250°F.